The BFS/HL sorbent was prepared at a weight ratio of 30/70 with a slurrying time of 16h and a slurrying temperature of 65℃.
炉石/氢氧化钙吸量配比为30/70,于65℃浆化16小时后乾燥后研磨制备而成。
The BFS/HL sorbent was prepared at a weight ratio of 30/70 with a slurrying time of 16h and a slurrying temperature of 65℃.
炉石/氢氧化钙吸量配比为30/70,于65℃浆化16小时后乾燥后研磨制备而成。
slurrying machinery: milling vessel, water pump, pipe and motor.
制浆机:由搅拌容、水泵、管道和电机组成。