Nanometer sized lead oxide was prepared by pyrogenetic decomposition of lead carbonate synthesized by chemical precipitation.
采用均匀沉淀法合成碳酸铅,在此基础上通过高温分制备纳米氧化铅。
Nanometer sized lead oxide was prepared by pyrogenetic decomposition of lead carbonate synthesized by chemical precipitation.
采用均匀沉淀法合成碳酸铅,在此基础上通过高温分制备纳米氧化铅。